Material: TP316L UNS S31603
OD: 5/8" or 0.625"
Chemistry Composition
C,% 0.035 max Mn,% 2.00 max P,% 0.045 max S,% 0.030 max Si,% 1.00 max Cr,% 16.0-18.0 Ni,% 10.0-14.0 Mo,% 2.00-3.00
Mechanical Properties
Tensile Strength: 70,000psi (483MPa) min
Yield Strength: 40,000psi (276MPa) min
Hardness: 192HBW, 200HV or 90HRB max
Tensile strength & yield strength minimum are calculated on specified wall.
Other dimensions are available on request. |