JIS G3462 Alloy steel boiler and heat exchanger tubes
Standard: JIS G3462
Equivalent Standards: ASTM A213, ASTM A335, EN 10216-2, DIN 17175, BS 3059, BS 3606, ISO 9329-2, ISO 9330-2, BS 3604, DIN 17176
Material: STBA 26
Equivalent Material: T9, 622-490, P9, 12Cr9Mo, X12CrMo9-1, 629, 1.7386, X11CrMo9-1
Chemistry Composition
C, %
Si, %
Mn, %
P, %
S, %
Cr, %
Mo, %
0.15 max
0.25-1.00
0.30-0.60
0.030 max
0.030 max
8.00-10.0
0.90-1.10
Mechanical Properties
Tensile Strength , MPa
Yield Strength, MPa
Elongation, %
Hardness, HRB
410 min
205 min
30 min
89 max
Outside Diameter & Tolerance
Hot rolled
Outside Diameter, mm
Tolerance, mm
OD<100
+0.4/-0.8
100≤OD<160
+0.4/-1.2
160≤OD<200
+0.4/-1.8
OD≥200
+0.4/-2.4
Cold Drawn
Outside Diameter, mm
Tolerance, mm
OD<25
±0.10
25≤OD<40
±0.15
40≤OD<50
±0.20
50≤OD<60
±0.25
60≤OD<80
±0.30
80≤OD<100
±0.40
100≤OD<120
+0.40/-0.60
120≤OD<160
+0.40/-0.80
160≤OD<200
+0.40/-1.20
OD≥200
+0.40/-1.60
Wall thickness & Tolerance
Hot rolled
Outside Diameter, mm
Tolerance, %

OD<100, WT<2.0

-
OD<100, 2.0≤WT<2.4
+40/-0
OD<100, 2.4≤WT<3.8
+35/-0
OD<100, 3.8≤WT<4.6
+33/-0
OD<100, WT≥4.6
+28/-0
OD≥100, WT<2.0
-
OD≥100, 2≤WT<2.4
-
OD≥100, 2.4≤WT<3.8
+35/-0
OD≥100, 3.8≤WT<4.6
+33/-0
OD≥100, WT≥4.6
+28/-0
Cold Drawn
Outside Diameter, mm
Tolerance, %
OD<40, WT<2.0
+0.40mm/-0mm
OD<40, WT≥2.0
+20/-0
OD≥40
+22/-0
JIS G3462 specifies alloy steel tubes used for heat transfer, for instance, water tubes, smoke pipe, superheater tube, air preheater tube, heat exchanger tubes, condenser tubes which are widely used in the chemical and petroleum industry. JIS G3462 usually applies to tubes with an outer diameter of 15.9mm to 139.8mm.
Manufacture: tubes to JIS G3462 shall be manufactured by hot rolled or cold drawn process.
Heat Treatment: full or isothermal anneal, normalize and temper.
Inspection & Test: chemistry composition analysis, tensile test, hardness test, flattening test, flaring test, NDT, surface inspection and dimension check.
Length: 5800mm; 6000mm; 6096mm; 7315mm; 11800mm; 12000mm; and so on.
Max developed length: 30 meters, also U bending, finning, studded process can be provided.
Option: shot blasting on the outside surface to remove mill scale, make the surface matte colour; surface polishing as preparation work done for further processing, for instance finning.
Keyword: JIS G3462, ASTM A213, ASTM A209, EN 10216-2, DIN 17175, BS 3059, BS 3606, Heat Exchanger Tubes